Its supposed to help dissipate the heat from the sparkplugThe Spyder shop manual calls for heat-sink paste to be applied to new spark plugs. Some Spyder dealers seem to be ignoring this requirement and their parts departments don't stock the stuff.
Are you using heat-sink paste?
Dealers that do not use the paste are not following the Service Manual procedure, which calls for the application of P12 heat-sink paste (P/N 420897186).
-Scotty![]()
I have not had to change plugs in the Spyder yet, but I will use the paste. There is usually a good engineering reason for specifying things like this. Most stem from problems discovered during prototype testing. On some engines a heat-sink paste or anti-seize compund also keeps the plugs from seizing in the alloy heads. I will do whatever BRP requires as long as the Spyder remains under warranty, even if I think it is overkill.Scotty: Do you use this - yourself?
There are a number of things in the maintenance schedule and shop manual that I choose not to do. I don't know if heat-paste will be one of them. It would be helpful to know what the consensus is in the Spyder community.
I have not had to change plugs in the Spyder yet, but I will use the paste. There is usually a good engineering reason for specifying things like this. Most stem from problems discovered during prototype testing. On some engines a heat-sink paste or anti-seize compund also keeps the plugs from seizing in the alloy heads. I will do whatever BRP requires as long as the Spyder remains under warranty, even if I think it is overkill.
-Scotty![]()
That would be my guess, but there are other considerations. A metallic compound can increase or even cause electrolysis. I think it is better to go with what the manufacturer uses, and has tested. Not sure of the cost of the BRP stuff, but one tube or jar should last you a lifetime.Aren't most anti-sieze compounds high in metal content and are going to behave like a heat sink compound anyway?.......Is there any difference :dontknow:
Just trying to avoid having to buy the BRP stuff.
What is the difference between heat sink and high temp anti-sieze paste. I have used anti-sieze for years in aluminium heads with no trouble. The BRP stuff must be expensive, I'm sure.
OK, tracked this stuff down.
:lecturef_smilie:
The heat sink paste is made by Wacker Chemie AG and is otherwise known as Wacker Silicone Heat Sink Paste P12
This same stuff is also specified for all Rotax aircraft engines.
It's also commonly used by Electronics manufactuers as a heat sink paste.
It's a pure silicone grease (polysiloxone) with suspended ceramic particles (most likely zinc oxide though they're not giving away that information). Thus it is chemically neutral and does not conduct electricity. It is used specifically to better transfer heat from the plug to the head by filling the gaps in the theads and providing a larger contact patch to conduct heat.
It is not the same as an anti-sieze compound, most of which are made of various metal compounds in a petroleum based grease. They are designed to allow the grease to vaporize and leave behind the lubricating metal compounds.
I guess I'm going to have to break down and order a tube from my dealer :sour: though Radio Shack's Heat Sink Grease is also pure silicone with Zink Oxide but who knows how the formulations might differ.......still in a pinch it would probably work.
You didn't retire...you just started working on your own stuff instead of your employer's.Retired engineer - thought this stuff was behind me - never would have to think about it again.
:agree::ani29:You didn't retire...you just started working on your own stuff instead of your employer's.We've seen your handywork.
-Scotty![]()